Physical Properties |
Metric |
English |
Comments |
Density |
1.95 g/cc |
0.0704 lb/in³ |
Water Absorption at Saturation |
0.0200 % |
0.0200 % |
Linear Mold Shrinkage |
0.00200 - 0.00600 cm/cm |
0.00200 - 0.00600 in/in |
Linear Mold Shrinkage, Transverse |
0.00300 - 0.00700 cm/cm |
0.00300 - 0.00700 in/in |
|
Mechanical Properties |
Metric |
English |
Comments |
Tensile Strength at Break |
115 MPa |
16700 psi |
Elongation at Break |
1.00 % |
1.00 % |
Flexural Modulus |
18.0 GPa |
2610 ksi |
Flexural Strength |
190 MPa |
27600 psi |
Izod Impact, Unnotched (ISO) |
15.0 kJ/m² |
7.14 ft-lb/in² |
Izod Impact, Notched (ISO) |
6.00 kJ/m² |
2.86 ft-lb/in² |
|
Electrical Properties |
Metric |
English |
Comments |
Volume Resistivity |
>= 1.00e+17 ohm-cm |
>= 1.00e+17 ohm-cm |
Surface Resistance |
>= 1.00e+15 ohm |
>= 1.00e+15 ohm |
Dielectric Constant |
5.20 @Frequency 10000 Hz |
5.20 @Frequency 10000 Hz |
Dielectric Strength |
25.0 kV/mm |
635 kV/in |
Dissipation Factor |
0.00100 @Frequency 10000 Hz |
0.00100 @Frequency 10000 Hz |
Comparative Tracking Index |
175 V |
175 V |
|
Thermal Properties |
Metric |
English |
Comments |
CTE, linear |
19.0 µm/m-°C @Temperature 20.0 °C |
10.6 µin/in-°F @Temperature 68.0 °F |
CTE, linear, Transverse to Flow |
24.0 µm/m-°C @Temperature 20.0 °C |
13.3 µin/in-°F @Temperature 68.0 °F |
Melting Point |
280 °C |
536 °F |
Deflection Temperature at 1.8 MPa (264 psi) |
270 °C |
518 °F |
Glass Transition Temp, Tg |
90.0 °C |
194 °F |
|
Processing Properties |
Metric |
English |
Comments |
Melt Temperature |
310 - 340 °C |
590 - 644 °F |
Mold Temperature |
135 - 160 °C |
275 - 320 °F |
Drying Temperature |
135 °C |
275 °F |
Dry Time |
3 - 4 hour |
3 - 4 hour |