Physical Properties |
Metric |
English |
Comments |
Density |
1.76 g/cc |
0.0636 lb/in³ |
Water Absorption |
<= 0.0400 % |
<= 0.0400 % |
Linear Mold Shrinkage |
0.0200 - 0.0300 cm/cm |
0.0200 - 0.0300 in/in |
Melt Flow |
5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
15.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
15.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Mechanical Properties |
Metric |
English |
Comments |
Hardness, Shore D |
63.0 @Thickness 2.00 mm |
63.0 @Thickness 0.0787 in |
Tensile Strength, Ultimate |
14.0 - 30.0 MPa |
2030 - 4350 psi |
Tensile Strength, Yield |
14.0 - 35.0 MPa |
2030 - 5080 psi |
Elongation at Break |
350 - 600 % |
350 - 600 % |
Elongation at Yield |
10.0 - 12.0 % |
10.0 - 12.0 % |
Modulus of Elasticity |
0.800 GPa |
116 ksi |
Flexural Modulus |
0.850 GPa |
123 ksi |
Flexural Yield Strength |
33.0 MPa |
4790 psi |
Coefficient of Friction |
0.200 - 0.300 |
0.200 - 0.300 |
Coefficient of Friction, Static |
0.200 - 0.400 |
0.200 - 0.400 |
Taber Abrasion, mg/1000 Cycles |
5.00 - 15.0 |
5.00 - 15.0 |
Izod Impact, Notched |
5.20 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
9.74 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
|
Electrical Properties |
Metric |
English |
Comments |
Electrical Resistivity |
>= 1.00e+14 ohm-cm |
>= 1.00e+14 ohm-cm |
Surface Resistance |
>= 1.00e+14 ohm |
>= 1.00e+14 ohm |
Dielectric Constant |
7.00 @Frequency 1e+6 Hz |
7.00 @Frequency 1e+6 Hz |
|
Thermal Properties |
Metric |
English |
Comments |
Heat of Fusion |
32.0 J/g |
13.8 BTU/lb |
|
34.0 J/g |
14.6 BTU/lb |
CTE, linear |
130 - 150 µm/m-°C @Temperature 20.0 °C |
72.2 - 83.3 µin/in-°F @Temperature 68.0 °F |
Specific Heat Capacity |
1.20 J/g-°C |
0.287 BTU/lb-°F |
|
1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
Thermal Conductivity |
0.180 W/m-K |
1.25 BTU-in/hr-ft²-°F |
Melting Point |
169 °C |
336 °F |
Crystallization Temperature |
127 °C |
261 °F |
Maximum Service Temperature, Air |
320 - 350 °C |
608 - 662 °F |
Deflection Temperature at 0.46 MPa (66 psi) |
82.0 °C @Thickness 4.00 mm |
180 °F @Thickness 0.157 in |
Deflection Temperature at 1.8 MPa (264 psi) |
48.0 °C @Thickness 4.00 mm |
118 °F @Thickness 0.157 in |
Vicat Softening Point |
140 °C @Load 1.00 kg, Thickness 4.00 mm |
284 °F @Load 2.20 lb, Thickness 0.157 in |
Brittleness Temperature |
-30.0 °C |
-22.0 °F |
Glass Transition Temp, Tg |
-30.0 °C |
-22.0 °F |
Oxygen Index |
46.0 - 65.0 % @Thickness 3.00 mm |
46.0 - 65.0 % @Thickness 0.118 in |